ABSTRACT

Water which used for the mix and curing in this work was tap water from the water-supply network system. Glenium-type 51 was used as super plasticizer.

Finely, crushed limestone was used as filler in this work, the mother rock of this filler was brought from the west desert of Iraq. The fineness of it can be described as 70% passing through sieve size 0.15 mm, and 30% passing through sieve size 0.075 mm.