chapter  6
38 Pages

Alpha + Beta Alloys*

Ti-6Al-4V, 960˚C/1h/WQ + 535˚C/6h/AC, tensile tested at room temperature. Low-magnification fractograph showing cup-and-cone fracture with a prominent shear lip. The high magnification photographs of regions A and B are shown in Figure 6.3 and Figure 6.4, respectively.