It was likely that corrosion occurred mainly at the cracked section of specimens, and concrete surface of some specimens were stained with red rust. Corrosion pattern depended on quality of concrete. Though corrosion generally extended along longitudinal direction of bars for normal concrete, corrosion was relatively limited near cracked section for high-strength concrete.