ABSTRACT
CFRP grid were measured near the crossing points on the grid (grid points) which have a laminated structure. Eight AE sensors were attached to the surface of the specimen as shown in Figure 1.
3 RESULTS AND DISCUSSION
3.1 Failure mode and crack pattern
Table 2 shows the failure mode and ultimate load for all specimens. Three failure patterns were observed in the experiment.