ABSTRACT

Figure 2 presents the variation of the modulus of elasticity (in percent of the initial value) versus the temperature. As per compressive strength, after heating to temperature of 800°C residual modulus of elasticity of dolomite based mixture is higher (19%) than in the case of all slag based mixtures (0-8.5%).