ABSTRACT

Rate of reduction of shrinkage strain at 91-day is shown in Figure 7. The amount of shrinkage reduction at 91-day is the difference between measured shrinkage strains and that of control specimen SFLC. Shrinkage reduction of specimen SFLC-G20 with aggregate replaced 20% with the porous ceramic waste was greater than that with expansive additive.