ABSTRACT

The dielectric properties that we have discussed so far mainly consider the influence of temperature and frequency on ε′ and ε″ and relate the observed variation to the structure and morphology by invoking the concept of dielectric relaxation. The magnitude of the macroscopic electric field that we considered was necessarily low since the voltage applied for measuring the dielectric constant and loss factor is in the range of a few volts.