ABSTRACT
Figure 117. Effect of Sm on tensile properties of the alloy Mg-5.5 mass % Gd at room temperature.
using hot extruded rods produced with a reduction area of about 90%. The rods were tested
in the "as extruded" condition and after additional ageing at 210°C for 36 h (T5 condition).
The results of the tests at room and elevated temperatures are presented in Table 37. They