ABSTRACT

After 28 days of hardening the decrease in compressive strength for specimens with 1% amount of emulsion was from 2.31 to 3.74% and for specimens with 15% amount of emulsion was from 56.19 to 67.33%. Decreases in compressive strength after 90 days were smaller-from 2.22 to 2.87% at 1% amount of emulsion and from 34.60 to 51.56% at 15% amount of emulsion.