ABSTRACT

The formation of both kinds of defects is an endoenergetic process and hence equilibrium constants Ks and KF', as well as the total concentrations of Schottky and Frenkel defects, increase with increasing temperature. It should here be observed that by appropriate cooling the equilibrated samples one can easily "freeze" the defect state corresponding to a high temperature.