ABSTRACT

The sensitivity to cracking was evaluated by means of the ASTM C 1581 ring test, which can take into account autogenous shrinkage effects which occur at a very early stage and also provide more meaningful characterization than the simple approach of evaluating free shrinkage. The latter does not take into account other parameters which control cracking such as the viscoelastic response and the rate of strength development.