ABSTRACT

As the test materials were used in this study, PCM based polyarylate DV [3] content of 50 percent powders of aluminum, iron (particle size 45 µ), nickel, copper (particle size 30 µ), tungsten (particle size 15 µ). The effectiveness of the explosive process is largely determined by the method of loading; therefore, the EC metal-filled polyarylate carried a moving shock wave (SW) in the plane loading with compaction pressure 0.67 GPA, which provides high-quality compacts. In order to achieve the required level of physico-mechanical properties of the treated metal-filled explosion polyarylate samples were sintered at a temperature of 260°C [4].