ABSTRACT

Abstract ................................................................................................... 44 4.1 Introduction .................................................................................... 44 4.2 Experimental Part ........................................................................... 49 4.3 Conclusions .................................................................................... 56 Keywords ................................................................................................ 57 References ............................................................................................... 57

ABSTRACT

The structure and physical properties of the thermoplastic vulcanizates produced in the process of the reactive processing of polypropylene and ethylene-octane elastomer in the form of alloy, using the cross-linking system was analyzed.