Figure 51 Effect of grain size on the creep strength of recrystallized lead-copper alloys at a stress of 2.1 MPa [2,191]. (Courtesy of Springer Verlag, New York.)
Figure 52 Variation of creep rates of commercial lead with Iff [2,199]. (Courtesy of Springer Verlag, New York.)
1 aOt a1 W
0.1 Average grain cross-section (mm2) 1.0
Figure 55 Lead with 64.5% Sn. Creep curves of cast and rolled sheets under tensile stress [2.201]. (Courtesy of Springer Verlag. New York.)
Figure 56 Effect of tin content on creep strength of specimens of similar grain size under a stress of 2.06 MPa [2.199]. (Courtesy of Springer Verlag. New York.)