ABSTRACT

Understanding the Basics of Nanoindentation and Why It Is ImportantContact damage induced brittle fracture is a common problem in the field of brittle solids. In the case of both glass and ceramics-and as it relates to both natural and artificial bio-materials-it has triggered the need for improved fabrication technology and new product development

chapter 1|10 pages

Contact Issues in Brittle Solids

ByPayel Bandyopadhyay, Debkalpa Goswami, Nilormi Biswas, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 2|10 pages

Mechanics of Elastic and Elastoplastic Contacts

ByManjima Bhattacharya, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 3|8 pages

Brief History of Indentation

ByNilormi Biswas, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 4|8 pages

Hardness and Elastic Modulus

ByNilormi Biswas, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 5|6 pages

Nanoindentation: Why at All and Where?

ByArjun Dey, Payel Bandyopadhyay, Nilormi Biswas, Manjima Bhattacharya, Riya Chakraborty, I. Neelakanta Reddy, and Anoop Kumar Mukhopadhyay

chapter 6|8 pages

Nanoindentation Data Analysis Methods

ByManjima Bhattacharya, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 7|4 pages

Nanoindentation Techniques

ByManjima Bhattacharya, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 8|6 pages

Instrumental Details

ByPayel Bandyopadhyay, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 9|16 pages

Materials and Measurement Issues

ByArjun Dey, Riya Chakraborty, Payel Bandyopadhyay, Nilormi Biswas, Manjima Bhattacharya, Saikat Acharya, Anoop Kumar Mukhopadhyay

chapter 10|8 pages

What If the Contact is Too Quick in Glass?

ByRiya Chakraborty, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 11|6 pages

Enhancement in Nanohardness of Glass: Possible?

ByRiya Chakraborty, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 12|12 pages

Energy Issues in Nanoindentation

ByRiya Chakraborty, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 13|12 pages

Dynamic Contact Damage in Glass

ByPayel Bandyopadhyay, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 14|8 pages

Does the Speed of Dynamic Contact Matter?

ByPayel Bandyopadhyay, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 15|10 pages

Nanoindentation Inside the Scratch: What Happens?

ByPayel Bandyopadhyay, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 16|6 pages

Nanomechanical Properties of Ceramics

ByRiya Chakraborty, Manjima Bhattacharya, Arjun Dey, and Anoop Kumar Mukhopadhyay

chapter 17|6 pages

Does the Contact Rate Matter for Ceramics?

ByManjima Bhattacharya, Riya Chakraborty, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 18|8 pages

Nanoscale Contact in Ceramics

ByManjima Bhattacharya, Riya Chakraborty, Arjun Dey, and Anoop Kumar Mukhopadhyay

chapter 19|6 pages

Shock Deformation of Ceramics

ByRiya Chakraborty, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 20|8 pages

Nanohardness of Alumina

ByRiya Chakraborty, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 21|8 pages

Interaction of Defects with Nanoindents in Shocked Ceramics

ByRiya Chakraborty, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 22|10 pages

Effect of Shock Pressure on ISE: A Comparative Study

ByRiya Chakraborty, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 23|6 pages

Nano-/Micromechanical Properties of C/C and C/C-SiC Composites

BySoumya Sarkar, Arjun Dey, Probal Kumar Das, Anil Kumar, and Anoop Kumar Mukhopadhyay

chapter 24|8 pages

Nanoindentation on Multilayered Ceramic Matrix Composites

BySadanand Sarapure, Arnab Sinha, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 25|10 pages

Nanoindentation of Hydroxyapatite-Based Biocomposites

ByShekhar Nath, Arjun Dey, Prafulla K. Mallik, Bikramjit Basu, Anoop Kumar Mukhopadhyay

chapter 26|6 pages

Nanoindentation of Silicon

ByArjun Dey, Anoop Kumar Mukhopadhyay

chapter 27|6 pages

Nanomechanical Behavior of ZTA

BySadanand Sarapure, Arnab Sinha, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 28|6 pages

Nanoindentation Behavior of Actuator Ceramics

BySujit Kumar Bandyopadhyay, A. K. Himanshu, Pintu Sen, Tripurari Prasad Sinha, Riya Chakraborty, Arjun Dey, Payel Bandyopadhyay, Anoop Kumar Mukhopadhyay

chapter 29|6 pages

Nanoindentation of Magnetoelectric Multiferroic Material

ByPintu Sen, Arjun Dey, Anoop Kumar Mukhopadhyay, Sujit Kumar Bandyopadhyay, A. K. Himanshu

chapter 30|8 pages

Nanoindentation Behavior of Anode-Supported Solid Oxide Fuel Cell

ByRajendra Nath Basu, Tapobrata Dey, Prakash C. Ghosh, Manaswita Bose, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 31|8 pages

Nanoindentation Behavior of High-Temperature Glass–Ceramic Sealants for Anode-Supported Solid Oxide Fuel Cell

ByRajendra Nath Basu, Saswati Ghosh, A. Das Sharma, P. Kundu, Arjun Dey, and Anoop Kumar Mukhopadhyay

chapter 32|4 pages

Nanoindentation on HAp Coating

ByArjun Dey, Payel Bandyopadhyay, Nil Ratan Bandyopadhyay, Anoop Kumar Mukhopadhyay

chapter 33|6 pages

Weibull Modulus of Ceramic Coating

ByArjun Dey, Anoop Kumar Mukhopadhyay

chapter 34|6 pages

Anisotropy in Nanohardness of Ceramic Coating

ByArjun Dey, Anoop Kumar Mukhopadhyay

chapter 35|6 pages

Fracture Toughness of Ceramic Coating Measured by Nanoindentation

ByArjun Dey, Anoop Kumar Mukhopadhyay

chapter 36|6 pages

Effect of SBF Environment on Nanomechanical and Tribological Properties of Bioceramic Coating

ByArjun Dey, Anoop Kumar Mukhopadhyay

chapter 37|8 pages

Nanomechanical Behavior of Ceramic Coatings Developed by Micro Arc Oxidation

ByArjun Dey, R. Uma Rani, Hari Krishna Thota, A. Rajendra, Anand Kumar Sharma, Payel Bandyopadhyay, Anoop Kumar Mukhopadhyay

chapter 38|6 pages

Nanoindentation Behavior of Soft Ceramic Thin Films: Mg(OH)2

ByPradip Sekhar Das, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 39|6 pages

Nanoindentation Study on Hard Ceramic Thin Films: TiN

ByArjun Dey, Anoop Kumar Mukhopadhyay

chapter 40|6 pages

Nanoindentation Study on Sputtered Alumina Films for Spacecraft Application

ByI. Neelakanta Reddy, N. Sridhara, V. Sasidhara Rao, Anju M. Pillai, Anand Kumar Sharma, V. R. Reddy, Anoop Kumar Mukhopadhyay, Arjun Dey

chapter 41|10 pages

Nanomechanical Behavior of Metal-Doped DLC Thin Films

ByArjun Dey, Rajib Paul, A. K. Pal, Anoop Kumar Mukhopadhyay

chapter 42|6 pages

Orientational Effect in Nanohardness of Tooth Enamel

ByNilormi Biswas, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 43|6 pages

Slow or Fast Contact: Does it Matter for Enamel?

ByNilormi Biswas, Arjun Dey, Anoop Kumar Mukhopadhyay

chapter 44|6 pages

Anisotropy of Modulus in Cortical Bone

ByArjun Dey, Himel Chakraborty, Anoop Kumar Mukhopadhyay

chapter 45|8 pages

Nanoindentation of Fish Scale

ByArjun Dey, Himel Chakraborty, Anoop Kumar Mukhopadhyay

chapter 46|8 pages

Indentation Size Effect (ISE) and Reverse Indentation Size Effect (RISE) in Nanoindentation

ByArjun Dey, Devashish Kaushik, Nilormi Biswas, Saikat Acharya, Riya Chakraborty, Anoop Kumar Mukhopadhyay

chapter 47|10 pages

Pop-in Issues in Nanoindentation

ByRiya Chakraborty, Arjun Dey, Manjima Bhattacharya, Nilormi Biswas, Jyoti Kumar Sharma, Devashish Kaushik, Payel Bandyopadhyay, Saikat Acharya, and Anoop Kumar Mukhopadhyay

chapter 48|8 pages

Effect of Loading Rate on Nanoindentation Response of Brittle Solids

ByRiya Chakraborty, Arjun Dey, Nilormi Biswas, Manjima Bhattacharya, Payel Bandyopadhyay, Jyoti Kumar Sharma, Devashish Kaushik, Saikat Acharya, and Anoop Kumar Mukhopadhyay

chapter 49|6 pages

Measurement of Residual Stress by Nanoindentation Technique

ByArjun Dey, Anoop Kumar Mukhopadhyay

chapter 50|8 pages

Reliability Issues in Nanoindentation Measurements

ByArjun Dey, Anoop Kumar Mukhopadhyay

chapter 51|6 pages

Substrate Effect in Thin Film Measurements

ByArjun Dey, I. Neelakanta Reddy, N. Sridhara, Anju M. Pillai, Anand Kumar Sharma, Rajib Paul, A. K. Pal, Anoop Kumar Mukhopadhyay

chapter 52|8 pages

Future Scope of Novel Nanoindentation Technique

ByArjun Dey, Anoop Kumar Mukhopadhyay