ABSTRACT

Attention was paid to the conditioning of the timber before and after the manufacture of the joints. The conditioning was conducted in such a way that the test conditions correspond in a realistic manner to adequate in situ conditions as regards the influence of moisture content and the occurrence of gaps induced by shrinkage.