ABSTRACT

If now the weldment is heated to 500-800°C for stress-relieving purposes or in service, chromium carbide forms and sensitization follows. Since niobium carbide needs a higher temperature to form, the presence of niobium in the alloy cannot prevent chromium carbide formation. The same situation prevails for the titanium-stabilized variety.