ABSTRACT
Although it was possible to fit appropriately with a suitable rheological model the response of the sample for the whole test, including the temperature steps, the value obtained for the Arrhenius’s coefficient, which reflects the effect of temperature on the viscoplastic strain was too high and was assessed to be not reliable.