ABSTRACT

Two types of superabsorbent polymers were used in cementitious composites (BASF). SAP 1 is a crushed type polymer with a lower affinity to water while SAP 2 has spherical shape particles. The w/c ratio in SAP containing mortar had to be adjusted to keep the same flow value, from 0.3 to 0.33 and 0.34.