ABSTRACT

Fe, 2 nm Au, 3 nm Fe and 4 nm Au. The SNR of the Fe L2,3-edge in the centre of

the 3 nm Fe layer is better than that from the 1 nm Fe layer owing to the limited

spatial resolution of the probe. This leads to a lower Fe signal on an increased

background.