ABSTRACT
Thermal and photo-oxidative degradation of polymers in the presence of
oxygen is accompanied by irreversible changes in their physical-mechanical
properties up to complete destruction. In order to prevent oxidation various
stabilization methods are used, which have been considered in Chapter 1.